Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® T6340G6 - PA66/6T-GF30 FR(40) - BASF

Material Data Center offers the following functions for Ultramid® T6340G6:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid T datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Partially aromatic polyamide, halogen-free flame-retardant, with good mechanical and dielectric properties in presence of humidity and at elevated temperatures. It is easily colorable and allows easy processing with low tool corrosion.
Markets & applications
Automotive: high-voltage connectors, e-mobility
E&E: Connectors, MCBs
Consumer goods
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 40 / * cm³/10min ISO 1133
Température 300 / * °C -
Charge 5 / * kg -
Retrait au moulage, parallèle 0.5 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.9 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 11000 / 9100 MPa ISO 527
Contrainte à la rupture 145 / 110 MPa ISO 527
Déformation à la rupture 2.5 / 3.3 % ISO 527
Module de flexion, 23°C 9000 / 8000 MPa ISO 178
Résistance à la flexion 230 / 185 MPa ISO 178
Résistance au choc Charpy, +23°C 65 / 62 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 50 / - kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 10 / 10 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 9 / - kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 280 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 257 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 275 / * °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 19 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 65 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-0 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Yellow Card disponible oui / * - -
Inflammabilité pr. épaisseur h V-0 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.4 / * mm -
Yellow Card disponible oui / * - -
Inflammabilité 5V pr. épaisseur h 5VA / * class IEC 60695-11-20
Epaisseur de l'éprouvette 1.0 / * mm -
Yellow Card disponible oui / * - -
Aptitude à l'allumage 45 / * % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.8 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.8 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (2) 1 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale 1E13 / 1E12 Ohm*m IEC 62631-3-1
Résistivité superficielle * / >1E15 Ohm IEC 62631-3-2
Rigidité diélectrique 40 / 36 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 / - - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 4.3 / * % Sim. to ISO 62
Absorption d'humidité 1.3 / * % Sim. to ISO 62
Masse volumique 1410 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 - 100 °C -
Pré-séchage - temps 4 - 8 h -
Température de la matière fondue 285 - 320 °C -
Température du moule 90 - 110 °C -
Fonctions
Module de cisaillement dynamique / Température , Ultramid® T6340G6 (sec), PA66/6T-GF30 FR(40), BASF
Module de cisaillement dynamique / Température , Ultramid® T6340G6 (cond.), PA66/6T-GF30 FR(40), BASF
Contrainte / Déformation , Ultramid® T6340G6 (sec), PA66/6T-GF30 FR(40), BASF
Module sécant / Déformation , Ultramid® T6340G6 (sec), PA66/6T-GF30 FR(40), BASF
Module de traction / Température , Ultramid® T6340G6 (sec), PA66/6T-GF30 FR(40), BASF
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent ignifugeant
Propriétés spéciales
Ignifugé, Sans halogène
Applications
Automobile, Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Autres informations
Moulages par injection
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 - 100 °C
Pre/Post-processing, Pre-drying, Time: 4 - 8 h

PROCESSING
injection molding, Melt temperature, range: 285 - 320 °C
injection molding, Melt temperature, recommended: 300 °C
injection molding, Mold temperature, range: 90 - 110 °C
injection molding, Mold temperature, recommended: 100 °C
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.